Friday, March 24, 2017

Re: [MW:26274] SA 387 Gr. 11

what is working temp for combination of 304+Gr11

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Thu, Mar 23, 2017 at 10:19 PM, dilintas <dilintas@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (dilintas@gmail.com) Add cleanup rule | More info

1. You can use it
2. 309L



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Materials & Welding <yudistira.dunggio@gmail.com>
Date: 23/03/2017 08:19 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26259] SA 387 Gr. 11

Hai All,

I'm knew in this group.
I believe many of you have many expereince in this situation.

I've been try to looking many refferences but still hard to find the right one.

my Problem are:

  1. with what method that I need to use when I want to Joint Plate for Type material like SA-387 Gr. 11 to SA 516 Gr. 70. and what kind of Electrode that I need to use? is it enough using ER 80S B2 in Gtaw?
  2. Similiar to question above, What Kind of method that I will use when want to join material Plate like SA240 Gr. 304H to SA-387 Gr. 11?

perhaps many of you can help me on this situation.

Thank you for your information on this

Warm regards
Yudistira

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/44bc1812-6180-4cf4-ad6f-aed21871075d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/etalxojgifeec5qr1ff1gw9l.1490287776746%40email.android.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN8A-N3cOhu7tzEnLbEGwd86YTNsoj3J6My_dMHyhzyFA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...