Wednesday, March 22, 2017

Re: [MW:26251] E6010 electrode for root



Dear Sir,

In process piping B 31.3 for larger dia we use E6010 for so many years. Fumes shall be safely exhausted.



Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +9184695933

Sent from RediffmailNG on Android




From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: Tue, 21 Mar 2017 16:27:30 GMT+0530
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:26238] E6010 electrode for root

no because it has got more H2 of 30to60ppm

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Mar 21, 2017 at 10:29 AM, ishwar kumar <ish8623@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (ish8623@gmail.com) Add cleanup rule | More info

Yes we can 

Sent from my iPhone

On 21-Mar-2017, at 12:39 AM, S.Mohammed <mohd52100@gmail.com> wrote:

Dear all,
Shall we used E6010 electrode for root for 31.3 process piping?
Is there restriction specifies in B31.3?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/CANX-_HGuYG7KiBuz4xc-9VhQJ%2BNNOANujkoLsgZDBGEgBjsQ0w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/21B46305-39B6-4FD8-B538-96EF51C12FDC@gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMpESBbrnZ=rQ1UPj6NfhwknB5MDbZqWL1Vza=RTSZH9g@mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1490164981.S.24066.autosave.drafts.1490165169.8505%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...