Dear sir,

You can avoid such type of issue by internal drawing study.

Secondly, Do the RT of the joint and make it flush and place a shoe support below it.
In second option, you can also cut the pipe and place a piece of pipe in between shoe.
In second case , your one extra joint will be created but no issue of failure in future.
In third option, you can shift the pipe and make the joint safe.


Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/13edc846-2123-4fff-992c-0d147ace233e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...