Dear All

1) Do the users/operators qualifies (or) accepts the use of CRA clad carbon steel line pipe in accordance with 811.2.4(a) of ASME B31.8 when the pipeline systems are designed in accordance with ASME B31.8?

2) What is the usual practice for use of CRA clad line pipe in accordance with API 5LD that is not defined under 814.1.1 of ASME B31.8?

Krishnnaa26







































































































































































































































































































































































































































































































































































































































































































































































































































































































--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/552641e8-d3c5-4626-b6dc-812856ea50e7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...