--Yes you can use a nitric solution for passivation to eliminate carbon pick-up.
Jim Price | Welding Engineer, CWI
Direct: 320.7463439 | Fax: 417-862-5564
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohit Aggarwal
Sent: Thursday, May 12, 2016 1:27 AM
To: materials-welding
Subject: [MW:24785] Regarding SS 304 Cleaning
Dear Experts,
Kindly let me know that If SS is effected by Carbon steel and surface get little effected, then is it right to clean it with Nitric Acid by dipping.
Regards,
Mohit Aggarwal.--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNOt0CCbV9uYQB7FC8oWU1vrx71_PgfXYnrn_Ab8kOb3w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d5383f90202b423c8d5c865cb3304320%40POLARMAIL.PolarTank.local.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO4Qa23zViHdsBtQ%3Dz8rs-pEXudsFaHSat1DwrViD5KLw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment