Acording to lSO 9606-1 point 6.1 it shall be done "yes"
On Sun, May 8, 2016 at 10:13 AM, Vijay Katkar <katkar.vijay22@gmail.com> wrote:
Do we need to appoint examinations body to quality each Welder as per ISO 9606?
On May 8, 2016 12:19 PM, "Prakash Gotimukul" <gprakash31@gmail.com> wrote:--Any notified body( NoBo) accredited to witness and certify welding procedures/welders--On Sat, May 7, 2016 at 8:02 PM, Vijay Katkar <katkar.vijay22@gmail.com> wrote:Dear All,
Need your help on below topic.
What is the meaning of Examiner and examination body as per ISO 9606?
What is the criteria for Examiner ?
Can person from organization consider as Examiner?
Thank you
Vijay Katkar
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrKAVmiocWBfyBzJJFg0%3D2K7wHycFyySazUUmehq9NOQjQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2Byo7D5JOJA_A6_s7pZopHLxGY21tqRaKGcs7TXb%3DADJQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrJ03V6aUf%3DkkgVA2UN%2BFhneJZJQyVC81z0KJVnXMTSETQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Best Regardes,
Eng:- Elsayed Elghareeb.
Dipl. Welding Engineer.
DSD-FERROMETALCO.
+2 0100 82 61 645.
Eng:- Elsayed Elghareeb.
Dipl. Welding Engineer.
DSD-FERROMETALCO.
+2 0100 82 61 645.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOCciGJiqeKuc30-4FzrA-6%3DERBnO3rCfUQ-N93qh3FY3U5S6A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment