Sunday, May 8, 2016

Re: [MW:24768] ISO 9606 (Welder Qualification)

Any notified body( NoBo) accredited to witness and certify welding procedures/welders

Rgds
Prakash Gotimukul
AIS, Consultant ASME/ISO/PEDlIBR
 Mob:+97152 979 5678

On Sat, May 7, 2016 at 8:02 PM, Vijay Katkar <katkar.vijay22@gmail.com> wrote:

Dear All,

Need your help on below topic.

What is the meaning of Examiner and examination body as per ISO 9606?

What is the criteria for Examiner ?

Can person from organization consider as Examiner?

Thank you

Vijay Katkar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrKAVmiocWBfyBzJJFg0%3D2K7wHycFyySazUUmehq9NOQjQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2Byo7D5JOJA_A6_s7pZopHLxGY21tqRaKGcs7TXb%3DADJQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...