Thursday, May 12, 2016

[MW:24781] FW: AWS - D1.1 presentation on changes to D1.1:2015

as received


 

The following page was added in the Standards tab of the AWS website: https://www.aws.org/standards/page/d1-1-2015-changes. On the page you can watch a video and receive a pdf of a presentation that goes through the major changes to D1.1 in the latest edition (2015).  This is a very thorough walk presentation and is helpful for anyone who asks "What is different in the 2015 code as compared to 2010?".

 


 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubki-qohmnA%3D0FD6nq3YCVkWpxaLVkR-XO7p%3DKQ42RiG6A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...