[MW:24764] Re: RT JOINT FILM SIDE SOURCE SIDE IQI

Because you not mention OD pipe, so I dont know which technique using.
For SWSI technique: No way to counter check.
For DWSI/DWDI, you can compare distance from 02 wire IQI at RT film and distance actual. If it's same. IQI at film side.




Vào 12:26:08 UTC+7 Thứ Hai, ngày 18 tháng 4 năm 2016, Mohd Siraj đã viết:
DEAR ALL,

IS THERE ANY WAY TO.FIND THAT RT IS TAKNE WITH IQI FILM OR SOURCE SIDE BY FILM ITSELF.
I KNOW LETTER F.
IS THERE ANY WAY TO COUNTER CHECK?

MAT CS AND SS THK 3.91 -7.11 PIPES.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/47ae6c75-5cf8-43f5-90b0-d26b3b9a231d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...