[MW:22680] RE: 22679] Lateral Expansion - High Alloy Impact test

Saravanan,
 
Lateral expansion is a measure of ductility in addition to absorbed impact energy(impact values). Austenitic alloys always fail in ductile mode , with very high impact strength. Higher the ductility more is the LE. As these alloys have an inherent ductile nature , causing high impact values, the other way screen them is though lateral expansion.
 
Please see the links below and also ASTM/ASME -A/SA-370.
 
Thanks
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Saravanan Sornam
Sent: Tuesday, January 06, 2015 2:58 AM
To: materials-welding@googlegroups.com
Subject: [MW:22679] Lateral Expansion - High Alloy Impact test

Dear Metallurgists ,

Could you please explain that,

why lateral expansion value of Min. 0.38 mm given in ASME Sec VIII Div I , UHA-51 for Charpy Impact Tests, instead of Joule Value for High Alloy steels like Duplex, Super Duplex etc.

What is the significance of Lateral expansion for such High Alloys.

Regards,
Saravanan.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkKr_DRJNkPC5H-5Wwj16i0KubE370PKEXtxOrgbdUFBTw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...