Today I went through one MTC review for ASME SA516 in Mfr shop (the end user is a refinery).

Where I found the Columbium 0.05. The table 1 of SA20 limits the columbium for heat analysis to Max 0.02% however the Note Dallows that to be 0.05%. based on an agreement between purchaser and supplier.

The vendor says they are purchaser and they have agreed with supplier so "it should be acceptable". They have purchased the material out of stock.

 

Could I ask your kind opinion about this? Can I accept the material?

 

More details:

There is no favour neither any objection about this requirement from client.

The purchaser field in the MTC says: "To whome so ever it may concern"

mfr has purchased the material from A Steel Trading Co.

The certificate is EN10204-3.2 witnessed by TPI.

The certification statement says " the material manufactured and tested according to the requirements specified in the order"

 
With Best Regards,
Umar Rashid Makrani, PMP® ,
 API653, NACE CIP-2, LEEA Registered Engineer.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKyj7YyrOGoZ6VsFipTE5jnWCbm-uihV8sDB80U6p0cP%3Dvg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...