Re: [MW:22727] Thin material welding

Welding done with seam welding process  and found lack of fusion ,visual is rejected. Now the client is insist us too do repair welding and the joint should be full penetration weld according to ASME B31.3 seam welding.
Since it is 3mm thick material we need to do high travel speed welding , can we use GMAW -STT  process?

P.NEILASHKUMAR 
Sent from my iPad
MOB : 966 535017935
            91+9952110791

On Jan 14, 2015, at 9:07 PM, 'c sridhar' via Materials & Welding <materials-welding@googlegroups.com> wrote:

In principle Possible. U can use pulsed TIG welding process with  same type
filler wire and  a lower size.

But u have not mentioned the type of defect in the weld for better guidance.
 
C Sridhar.

Please don't print this e-mail unless you really need to. Save the environment.




 


From: 'Neilashkumar' via Materials & Welding <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, 13 January 2015 11:44 PM
Subject: [MW:22721] Thin material welding

  Dear all,

We have a project for Seam Welding repairing work of Stainless steel
round duct piping for rubber finish building,details are as follows,
Total repairing welding length-500-550meter
Pipe material.    --EFW304/304LSS A240
Pipe thickness --below 3mm
Pipe size --0.75" -20"dia
Can you please tell me whether it is possible to do repair welding ? Method
to do repair weld.

P.NEILASHKUMAR
Sent from my iPad
MOB : 966 533098265
           91+9952110791


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/C90FF222-A0AB-466C-8E5C-313F24AFEBF2%40yahoo.com.



For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/679113474.573808.1421258825483.JavaMail.yahoo%40jws10938.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...