Dear experts,

Please clarify below questions.

Back Ground:

-       Applicable construction code: ASME Sec. VIII, Div.1

-       Material : SA516-70N (35mm)

-       Equipment's MDMT: -20

-       The client request that impact testing shall comply with the code of construction and in accordance with PED 97/23/EC Annex 1, Para 7.5.

 

Question 1):

Shall we have to perform the impact test on this material in accordance with PED requirement even impact test is exempted as per UCS-66, ASME Sec. VIII Div.1?

 

Question 2):

When the impact test is required as per PED, should we have to use WPS with applying all supplementary essential requirements for weld joint?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/59ddf4e5-821f-4c9c-b504-95902341d46a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...