[MW:22692] Flare Bevel Groove Joint

Hi Experts

As per AWS D1.1 2010, whether Flare Bevel Groove Joint is a CJP or PJP?  As per AWS A 2.4, the flare grove joint usually have a symbol of S(E), S represent the Distance of point of tangency to top member and E will be groove weld size. However in the IFC drawing we recieved , does not have any of S(E)?

Can you guys let me know whether it is PJP or CJP? Any clause in AWS or relevant code to support this? 