Friday, January 9, 2015

Re: [MW:22690] Re: Corrosion & Painting

Hi,

Since it is a humid condition, you can get the surface preparation done with water blasting machines. For persisting corrosion you need to carry out RCA.

Sent from my iPhone

On Dec 31, 2014, at 6:55, Jian Xu <leonxj87@gmail.com> wrote:

Dear,
 
Depend on your description, I can't tell which degree of corrosion in your plant, but I try to give you some advices.
 
First, try to find the root cause about corrosion, such as, whether it is materials selection issue, or the plant locate in coast, or not good insulation work, etc.
 
Second, according to accurate root cause, plant decide to do painting. Then, you should find the qualify supplier of painting, also, selection proper coating and  construction process is based on process service condition. So, clarify meeting of cross-displinary is necessary!
Good luck!
 
Leon

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a41d83bd-1bf2-49b3-ab72-3d7e5f9f585c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...