Re: [MW:22694] Hardness Value of Inconel 625

345 HV max

On 1 Jan 2015 08:11, "LALU RAJENDRAN" <lalucpt@gmail.com> wrote:
Dear Experts,

What is the hardness value of Inconel-625 (ASTM B444 UNS N06625)?


Regards,
LALU
LINKS MIDDLE EAST

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13t1W3GvM2xV6z3_D91J-DiUjTgwynS%3DL3qeCBOTPy2-Ng%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF7Kwvm24dhESxSdTshgQ%3D0iA6_ADGtYV-v1ahtZvpmNC69s%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...