Sunday, January 18, 2015

RE: [MW:22731] ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?

Hi PKM,
 
Please see the appropriate clause as stated below.This is in line with the recommendations of Mr. Bhatula. Note the acceptance is not flat across the board, it's subject to engineer's discretion also.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 

4.2.2.1, Previous Performance Qualification. Previous performance qualification tests of welders, welding operators, and tack welders that are properly documented are acceptable with the approval of the Engineer. The acceptability of performance qualification to other standards is the Engineer's responsibility, to be exercised based upon the specific structure, or service conditions, or both.



From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mbabur.bwp@gmail.com
Sent: Saturday, January 17, 2015 10:29 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:22730] ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?

Dear,
Each standards have scope and limitations so we fallow the standard instructions.
Seniors better know.
Regards,
Babur khan Lashari
Sent from my BlackBerry 10 smartphone.
From: Raghuram Bathula
Sent: Saturday, 17 January 2015 18:23
To: Materials-Welding
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:22729] ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?

The acceptability of performance qualification to other standards is the Engineer's responsibility, to be exercised based upon the specific structure, or service conditions, or both.

On 17 January 2015 at 18:00, PK M <pkmqaqc@gmail.com> wrote:

Dear Experts,


ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?


Thanks,


Pkm.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnvoFknLH9Jh%2B_igyfk5pUMjWZNhPi2ftvv6q803dpmOA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20150117152844.6000789.55815.3541%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...