Hi Amol,

answering the cold forming intermidiate HT question, it depends on the determined fibre elongation. If your sphere fibre elongation is 5% and less, only cold forming is required before welding and if your fibre elongation is above 5% cold forming and intermidiate HT shall be applied. It is also advised to determine if PWHT is required since you are dealing with critical material (SA 517 Gr. F). I recommend that you consult ASME code to determine the fibre elongation.

On Friday, January 2, 2015 at 10:26:08 AM UTC+2, amol wrote:

we have to make a sphere from crown petal construction.Material SA 517 Gr F. UTS 790-820MPa. cold forming will be done
whether this will require intermediate heat treatment to avoid formation of cracking?
If so when/at which stage of forming it has to be carried out?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2d7abe5d-42e4-4aba-aa01-5646ae0f1964%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...