[MW:22739] Re: Minimum leak path test

Dear All, 

how to calculate minimum leak path for tube to tube sheet mockup test
Tube Thk : 1.65 mm
Tube-sheet : 50 mm

please provide formula

Durgesh Gaonkar


On Monday, September 10, 2012 at 8:01:42 PM UTC+5:30, krishna mudhale wrote:
Dear experts,   How to calculate minimum leak path (MLP) for tube to
tube sheet joint,please give me refrence also .         Thanks &
regards- krishna mudhale.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5f001552-bdac-4cd5-a0b8-4ca8a3727a33%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...