Saturday, January 10, 2015

RE: [MW:22695] Hardness Value of Inconel 625

hi,
 
as per NACE MR0103-2005, it is 35HRC.
 
I have attached snapshot of the standard. Pls refer the attachment and correct me if i am wrong.
 
Regards
R Vairamuthu
 

 

Subject: Re: [MW:22691] Hardness Value of Inconel 625
From: nithindsilva4u@gmail.com
Date: Fri, 9 Jan 2015 08:32:05 +0400
To: materials-welding@googlegroups.com

Hi,

It is not specified in code, if you refer to shell MESC, it is 32 HRC.

Sent from my iPhone

On Dec 31, 2014, at 10:06, LALU RAJENDRAN <lalucpt@gmail.com> wrote:

Dear Experts,

What is the hardness value of Inconel-625 (ASTM B444 UNS N06625)?


Regards,
LALU
LINKS MIDDLE EAST

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13t1W3GvM2xV6z3_D91J-DiUjTgwynS%3DL3qeCBOTPy2-Ng%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8C9A76F0-AF96-4440-B2F7-A792B49DBB02%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...