You require to test for 4 bend,Chemistry at various levels from fusion line,This is in addition to hardness at cross section as per client requirement
Regards
Hegde Prakash
+918805593046
--------------------------------------------
On Mon, 19/1/15, VALTECH INDUSTRIES - FAROOQ <farooq@valtechindustries.com> wrote:

Subject: [MW:22736] OVERLAY WELDING QUALIFICATION
To: materials-welding@googlegroups.com
Date: Monday, 19 January, 2015, 3:43 PM9
















Dear Sir,

 

Please let me know what
are the test required for overlay welding of
Stellite-6 on Carbon
Steel Casting conforming to ASTM-A 216 Gr. WCB of Valve like
PT and Hardness as
per ASME Section IX

Please let me know
whether FUSION Test is required or not?

The
thickness of WCB Plate is 26mm and Overlaying welding is
single layer and
minium requirement of overlaying is 1.6mm after machining of
job.

  

REGARDS





 

 









--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at http://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAJKgbj7r6rBGs9Nr5MFcKbfCgAAAEAAAAEzpTUJGtftKtnHKNwtU8I8BAAAAAA%3D%3D%40valtechindustries.com.

For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1421678294.90667.YahooMailBasic%40web192701.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...