[MW:22781] Useing wrong Flux in welding with SAW

Dear Experts

Our production department used wrong Flux in welding with SAW process ,please give me idea about it

in WPS mentioned Lincoln 880M and they used Lincoln 880  ...material is API 5l X65 to API 5L X65.

please give a idea about this issue , and let me know if ASME section 9 has a way to confirm this issue .

Thanks

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b38a8775-3b41-4c96-9fcc-1902cc4408ea%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...