Re: [MW:22714] Impact Testing for Flanges

To fulfill the spec., the answer is YES.
To fulfill engineering sense, the answer is NO.

On Mon, Jan 12, 2015 at 2:42 PM, Raghavendra Kiran <email2ragkiran@gmail.com> wrote:
Dear Experts,
We have received some sour service flanges (NACE MR-0175), These flanges are impact tested at 20 degree Celsius by the manufacturer.
 
Our specification calls as below. 

" All Carbon steel materials of thickness greater than 12.7 mm must be impact tested at minus (-29 degree Celsius) in accordance with ASME B31.3 (para 323.3)"

The design temperature of the line is 50 degree Celsius.

Do i need to get the flanges tested at -29 degree Celsius to fulfill the specification.


Experts please advise.

Thanks,
Kiran



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8f7333c1-b1c2-4ecd-b005-04b09494cb68%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMttW3gZFcRUE9f1mweNFDvD%2B%2BJUQnksNQa7bUNBxpXPTsg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...