Dear Metallurgy Experts ,

With ref. to the above subject and the attached file ,

please let me know the GTAW Filler, to be used with sufficient Data.

It seems AWS Class ER70S-A1, SFA 5.28 is matching for mechanical properties, but i wanted to reconfirm with you.

Regards,
Saravanan,
Korea

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkKD_dg_%3DUeFxYHqY0%3DLjgDeGx9_ej8Sk96gvtbJZnsOJQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...