Tuesday, January 13, 2015

Re: [MW:22717] Re: Indication on RT after Clad Weld Overlay-625

Please attache the image.......
 
With Best Regards,
Shashank C Vagal

From: Agu Didie <didie.agu@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, 13 January 2015 7:55 AM
Subject: [MW:22716] Re: Indication on RT after Clad Weld Overlay-625

dear israr,

may i know what this type of material? piping, structure or etc? details pls.

On Sunday, December 14, 2014 at 5:15:13 PM UTC+8, israr wrote:
Dear Friends,

Could you Pls inform me about the attached RT film Photos are acceptable?
If acceptable or not acceptable which code I should Ref. 

The indications are found after cladding 
--
Israr Ahmed Noor Mohammed
+919930308261
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/890d71e8-f996-4a9c-b401-28cc2ece4936%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...