Dear Experts,
I am new in this group and very glad to see conversation regarding needfull and got required answer of any issues.
Now, I have facing one of issue, At present  working with  Indian railway project, thirt party is also there from client side. They does't know what the wps & pqr becoz. Wps & PQR  is not mentioned in their spec./manual. But as per IS standard testing they have carried.
But 2nd authority is saying make wps & pqr.
Now question is...  whats the parameter to be set for rail section? Because all parameter are different from piping or structure. Whats format as per section IX or ...?
Mat. Spec. .. IR  T12 grade 880, 60kg 90 uts
Requesting all of you, Please advice and send a sample wps & pqr  as per this mat. Spec.

Regards,
Shakeel Ahamad

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHO2htLKrijmH257AJJnzQqHjH-Y_yWgfJwyY1u1s2UxybdLPw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...