Dear Kumar,

Have you calculated the leakage rate and temperature correction factor for the line under hydrotest.

Regards,

PARAG PANSARE.

On 25 Jul 2014 15:28, "Kumar" <sk7920541@gmail.com> wrote:

Dear all,
During the hydrotest of a product line of about 1.3 km (asme B31.3/4, 24 bar test pressure, 4 hour holding time), 2 blind flanges are given at each end. One of the flanges were found as leaking (as drops) upon inspection. Around 15 mtr. Of the line in between is underground and hidden as well. Sub-contractor is arguing that line has a pressure around 27 bar (due to temp.) Which is above test pressure thus can be accepted. They are saying code allows "blind flange leakage" also. Anyhow we are not agreeing for that. Expecting your valuable feedback on this issue.
Thanks in advance,
Kumar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...