Re: [MW:21420] Technical Query - Is it necessary to (RT) penalty/tracer for second time repaired welder?

Dear Pkm

Please refer interpretation 1-62 subject 336.5, Types & Extent of required examinations date issued 1982 june 9 file number 1578

Please look for answers in code interpretation questions. Q-1,2,3

Regards
Shridev

On 16 Jul 2014 05:44, "PK M" <pkmqaqc@gmail.com> wrote:

Dear Experts,


In accordance with ASME B 31.3 Para. 341.3.4 Progressive examination. if a welders weld is rejected and the repair is made by another welder, found defective again, repaired a second time and again found to be defective, is it necessary to RT  (Penalty/Tracer)  two additional sample for this repair welder (repair attended welder) ?


Regarding repairs the code state:

341.3.3 Defective Components and Workmanship.


An examined item with one or more defects (imperfections of a type or magnitude exceeding the acceptance criteria of this Code) shall be repaired or replaced; and the new work shall be reexamined by the same methods, to the same extent, and by the same acceptance criteria as required for the original work.

341.3.4 Progressive Sampling for Examination.


When required spot or random examination reveals a defect, then (a) two additional samples of the same kind (if welded or bonded joints, by the same welder, bonder or operator) shall be given the same type of examination 
(b) if the items examined as required by (a) above are acceptable, the defective item shall be repaired or replaced and reexamined as specified in para. 341.3.3, and all items represented by these two additional samples shall be accepted, but (c) if any of the items examined as required by (a) above reveals a defect, two further samples of the same kind shall be examined for each defective item found by that sampling (d) if all the items examined as required by (c) above are acceptable, the defective item(s) shall be repaired or replaced and reexamined as specified in para. 341.3.3, and all items represented by the additional sampling shall be accepted, but (e) if any of the items examined as required by (c) above reveals a defect, all items represented by the progressive sampling shall be either 
(1) repaired or replaced and reexamined as required, or
(2) fully examined and repaired or replaced as necessary, and reexamined as necessary to meet the requirements of this Code
(f ) If any of the defective items are repaired or replaced, reexamined, and a defect is again detected in the repaired or replaced item, continued progressive sampling in accordance with (a), (c), and (e) is not required based on the defects found in the repair. The defective item(s) shall be repaired or replaced and reexamined until acceptance as specified in para. 341.3.3. Spot or random examination (whichever is applicable) is then performed on the remaining unexamined joints.

 

Thanks,

Pkm..

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...