Re: [MW:21406] Re: AWS D1.1 and ASME Sect IX PQRs combinations

Establish both with ASME. Why AWS??
If P.No is issue for EH36, you can write only chemistry 


On Sun, Jul 13, 2014 at 6:54 PM, Naskabir Vengassery <naskabir@gmail.com> wrote:
Anban,
no code in  my knowledge address this matter .Hence such combination is technically not possible


On Thursday, June 26, 2014 2:03:44 AM UTC+3, Anban wrote:

Dear Experts

Dear Sirs

Pls advise .

AWS D1.1-Structural Welding Code-Steel
ASME IX - ASME Boiler & Pressure Vessel Code

Current situation- Module Tubular Columns( 800mm in dia x 30mm thk ) at assembly stage ( Vertical Position -Butt weld in 2G position ).
Material - AWS Group II- ASTM A131-Grade EH36
Internal accessibility - Not allowed for safety reasons.
So Project suggest to use- Root Run using GTAW and Fill/Cap by FCAW

I want to prepare WPS combining -
1- PQR qualified in 6G position using GTAW in accordance with ASME IX ( Base Material- APL 5L X65 ( CVN at -46 deg C)
2- PQR qualified in 2G position using FCAW( with ceramic  Backing Strip ) in accordance with AWS D1.1.( Base Material - AWS Group II-EH36-CVN at -40 deg C)

Can i do it? Does the codes prohibit such combinations? Is there any code Interpretations on this subject? 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...