[MW:21503] Re: difference between API 2W 50 and API 2W 50T

Both are very similar with min. yield stress of 50ksi (50T has higher range though 50-80ksi compared to 50-75ksi of 50). See more here

Cheers
ChemKB

On Thursday, July 24, 2014 3:44:01 AM UTC-5, prabuharan marimuthu wrote:
Hi all, 

May someone clarify me what are the difference between API 2W 50 and API 2W 50T because both of them looks similar to me.


Thank You

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...