Sunday, July 27, 2014

[MW:21478] Re: Initial prodution weld RT after WQT.


Hello,
 
As per QW-301.2 need production joint and as per QW-304.1 minimum 150mm length of the first production weld(s) made by welder may be examined by volumetric NDT.
 
 
On Friday, July 25, 2014 8:46:14 AM UTC+3, S.Mohammed wrote:

Dear all

Is there any where mentioned in ASME that we have to take initial prodution joint RT TWO or FIVE joint after Welder qualifition passed.

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...