Hello, dear colleagues. I hope all you are well

I have to inspect a pressure vessel as a welding inspector, and there are some surface imperfections on the head surface of this equipment. 
There is not any supplementary requirements. Only ASME rules. 
If we read ASME SA20, we have to repair injurious surface defects, as transcripted below. 


ASME SA20

9. Quality
9.1 General—Plates shall be free of injurious defects and
shall have a workmanlike finish.
9.2 Surface Imperfections:
9.2.1 For plates produced from plate-as-rolled, all injurious
surface imperfections shall be removed by the manufacturer.
..........

But how to identify injurious defects? I understand injurious as something that cause damage to its operations and do not understand it as injurious only if it is a esthetic defect. 

All opinions, orientations and considerations will be very helpful. 

Best regards, 

Fernando Lescovar Neto from Brazil
Marine Engineer - International welding Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...