Yes it will affect the hardness of the material.By grinding 2-3 mm its hardness will reduced.
 
Regards
Abhishek Singh
On Tuesday, July 15, 2014 11:41:33 AM UTC+5:30, dhirajdhomne wrote:
Dear Sir

Please guide does sample drawn by gas cutting change properties of sample which affect result in physical and chemical properties.

Most of manufacturers use this practice in stock of raw material (plate, angles, TMT bars)

Regards
Dhiraj Dhomne

  

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...