Hello Sam,
 
A quick response to your query.Please the salient differences between F53 and F51 as attached. Although both alloys are classified under P-10H, Gr-1. Sec-IX , equivalency formula does not always work for DSS/SDSS.This is due to the facts  that these alloys are  always used in services, where common materials fail.
 
What're the design requirements?? Is there a requirement of ASTM G48A Pitting corrosion test, ASTM -262,IGC test??Is so what practice?
 
Appreciate your response.
 
Thanks
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada

 

 

SA-182 F53 – Grade--S32750-UTS- 116 (800)-P.No- 10H Gr No-1 - 25Cr–7Ni–4Mo–N, Forgings

SA-182 F51 – Grade--S31803-UTS- 90 (620)- P No-10H Gr No-1 - 22Cr–5Ni–3Mo–N, Forgings

 



dear all, 

i am reviewing WPS/PQR for SDSS production welding of A182 F53 material as per Section IX. it is for 3/4" valve body to flange.

1) Valve manufacturer has submitted WPS/PQR of only DSS which is between A182 F51 (P no. 10H) to A890 4A (P no. not available). Also in wps it mentions No any P number available for           A890 4A. 
    can i accept this WPS/PQR for welding Super duplex SS while there is huge difference between their chemical properties ? can i accept WPS while one material without P number ? can u           please provide section IX clause if it accepts WPS material without P number.

2) same job will be done with backing strip which will be removed by machining after welding. requirement is 100% RT. my question is this RT shall be done after baking strip removal or before ?

thanks in advance for your reply.

regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...