dear all,

we are trying to only repair gate valve wedge's hardfaced area (which contacts with seat rings) of 8" gate valve.  wedge material is carbon steel (A216 WCB). wedge harfaced area became less thick due to wear.

1) can we remove original overlay and apply 13%chrome overlay ? in this case which welding rod should we apply. if yes can you please send me WPS for this ?

2) we can not able to trace the original harfaced material b'se it is old valve. PMI  is showing Ni- 51% , Fe-25% and Cr- 18 %. what is this material ?

your urgent reply is appreciated.

thanks,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...