Anban,
no code in  my knowledge address this matter .Hence such combination is technically not possible


On Thursday, June 26, 2014 2:03:44 AM UTC+3, Anban wrote:

Dear Experts

Dear Sirs

Pls advise .

AWS D1.1-Structural Welding Code-Steel
ASME IX - ASME Boiler & Pressure Vessel Code

Current situation- Module Tubular Columns( 800mm in dia x 30mm thk ) at assembly stage ( Vertical Position -Butt weld in 2G position ).
Material - AWS Group II- ASTM A131-Grade EH36
Internal accessibility - Not allowed for safety reasons.
So Project suggest to use- Root Run using GTAW and Fill/Cap by FCAW

I want to prepare WPS combining -
1- PQR qualified in 6G position using GTAW in accordance with ASME IX ( Base Material- APL 5L X65 ( CVN at -46 deg C)
2- PQR qualified in 2G position using FCAW( with ceramic  Backing Strip ) in accordance with AWS D1.1.( Base Material - AWS Group II-EH36-CVN at -40 deg C)

Can i do it? Does the codes prohibit such combinations? Is there any code Interpretations on this subject? 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...