Dear Alberto,

Hydro testing is used not only to check pressure resistance of the welds & welded material but also used for design validation ie all design parameters. So as per above we need to install permanent blind flange also for hydro testing.

Thanks & Regards
Mohan Kumar


From: "Alberto Bertoni" <alberto.bertoni@racine.ra.it>
Sent: Sat, 15 Feb 2014 10:44:14
To: materials-welding@googlegroups.com
Subject: R: [MW:20105] Hydrotest of Blind Flange
Dear Richard,
Hydrotest purpouse is for pressure resistance of the welds and welded materials (I,ve seen personally wrought materials fittings failing under hydro) therefore you do not need to install permanent blind flanges (and even original gaskets and bolts) as called by the ISO.
After hydrotest and assembly of the complete lines (spools, gaskets, bolts, inline items, valves, etc.) It could be advisable to perform a complete circuit leakage test with air or nitrogen to assess the corrent assembly of the bolted components, including also a bolt torque campaign with wrenches or special tools for bolts diameter > 1-1/2".

Regards,
Alberto
Alberto Bertoni

From: Richard robes <mech.processes@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Fri, 14 Feb 2014 18:34:39 -0800 (PST)
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:20101] Hydrotest of Blind Flange

Dear Experts,

Kindly comment on the issue - In ISO drawing there is a blind flange coming after weld neck flange and it's included in hydro test limit too. But now hydro test crew want to use temporary blind flange instead of permanent blind flange. My question is whether i have to include permanent blind flange during the hydro test.

Regards
Richard

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...