Re: [MW:20181] TICKNESS OF CONFINED MATERIAL.

Dear Ferguson Duru, with an ultrasonic thickness gauge machine your concern would be solved.

Regards,

Chukwumaobi Onwunaka

Sent from Yahoo Mail on Android



From: Ferguson Duru <fergiedimedici@gmail.com>;
To: <materials-welding@googlegroups.com>;
Subject: [MW:20177] TICKNESS OF CONFINED MATERIAL.
Sent: Tue, Feb 25, 2014 9:30:12 PM

HELLO EXPERTS.
PLEASE I NEED INFORMATION ON HOW TO GET AN INSTRUMENT THAT CAN MEASURE THE THICKNESS OF A MATERIAL FROM JUST ONE SIDE LIKE THE TICKNESS OF THE STEEL PLATE OF A PETROLEUM STORAGE THANK.
I WILL LIKE TO KNOW THE BRAND NAME AND POSSIBLY A LINK TO GET ONE.
 I HAVE SEARCHED THE INTERNET BUT HAVENT REALY GOT WHAT I NEED.
THANKS

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...