Sunday, February 23, 2014

Re: [MW:20168] UNS 6625 AND UNS 8904

Dear sir, 

thanks for your valuable reply.

i have the WPS for UNS no 6625 , can i qualify the the welder by using this WPS for UNS no 8904 material


Thanks & Regards,

Manikandan N

QC - Welding Inspector.
P O BOX  No : 1884                      
Trags - Doha                        

Mobile : +974 33982954  &  E-mail : manikandan@tragsqatar.com




On Sun, Feb 23, 2014 at 11:06 AM, Himan Nikdin <himan.nikdin@outlook.com> wrote:
Hi
Dear Mani

UNS 6625 is Ni-Base alloy and  is an excellent general purpose material for elevated temperature use in applications where high strength and a good oxidation resistance is needed. It has an excellent corrosion resistance in wide range of severe corrosive environments and it has very low tendency to localized corrosion in chloride containing environments. Ralloy 9982 fulfills ASTM B 834.


UNS 8904  is an austenitic stainless steel with superior corrosion resistance in comparison with Type 316L and Type 317L. Due to addition of Cu (1.5%), this material displays excellent corrosion resistance against reducing acids such as sulfuric acid and phosphoric acid. It is used in chemical plants and a wide range of other applications. Nippon Yakin supplies this product in plate, sheet and strip form.


Regards,
Himan Nikdin


Date: Sun, 23 Feb 2014 10:29:05 +0300
Subject: [MW:20163] UNS 6625 AND UNS 8904
From: manigdcl@gmail.com
To: materials-welding@googlegroups.com

Dear Sir,

i need to confirm, UNS 6625 and UNS 8904 materials are equivalent. or not

pls give me the details...

Thanks & Regards,

Manikandan N

QC - Welding Inspector.
P O BOX  No : 1884                      
Trags - Doha                        

Mobile : +974 33982954  &  E-mail : manikandan@tragsqatar.com



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...