Re: [MW:20166] Tube to Tubesheet Expansion Mockup

First, it is non mandatory appendix.
Second it is only applicable for select cases (Read A1 starting clauses)
What is use of procedure, if you don't do mockup?


On Sat, Feb 22, 2014 at 6:20 PM, Josnit <nithindsilva4u@gmail.com> wrote:

Dear Experts,


With reference to Non mandatory appendix A (A-1(f)) of ASME Section VIII Div.1 & Annex 4-C (4-C.1.6) of ASME Section VIII Div.2,

 

Does these para’s speaks about tube to tubesheet expansion mock up procedure or mock up records need to be established and submitted for AI review? Please clarify.

 

If it is mock up records, then requesting you to forward sample records with respect to ASME Section VIII Div.1 & Div.2. 


Regards,

Josnit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...