Re: [MW:20157] RE: Black spots on DSS Weld Joints.

Dear Friends ,

We had the same problem for tig (gtaw) , as we realised that all black spots were small slag zones , the solution was grinding before pickling will exactly solve your problem if there aren't any other problems or mistakes

Best Regards

>Tahir Bilge Olmez
>International Welding Eng.
>Met. & Mat Eng.
>Verify Europe & Atlantic Marine Survey
>+90 544 6158801

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...