Thursday, February 20, 2014

Re: [MW:20151] roll bending of sa517 plate

You may try the info in the attachment.
As regards your question, thickness and ductility matter amongst other parameters
 
With Best Regards,
Shashank Vagal


On Sunday, 15 December 2013 1:14 PM, "saba.degheh@gmail.com" <saba.degheh@gmail.com> wrote:
I'm a university student and I'm working on a pressure vessel fabrication, I want to know how should I design the bending process and which codes and standards should I refer to?
Is it possible to make a 3 meters diameter shell from a welded SA517 plate in quenched and tempered condition? 
 thanks
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...