Tuesday, February 18, 2014

Re: [MW:20132] Stabilizing Heat Treatment of SS 321

We need to create titanium carbide to make steel capable to eliminate sensitizing at 450 to 780 deg range.


-----Original Message-----
From: CHINTUKUMAR GANDHI <cgandhi1975@yahoo.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Sun, Feb 16, 2014 4:19 pm
Subject: [MW:20112] Stabilizing Heat Treatment of SS 321

Dear Experts,

In one of our client project spec., it is specified that SS 321 pipes shall be in a stabilized HT condition. Stabilizing HT shall be carried out subsequent to the normal solution annealing. Soaking temp. & holding time for stabilizing HT shall be 900º C & 4 hrs respectively.

My questions are (1) what is the purpose of stabilizing HT (2) This stabilized HT pipe shall be solution annealed after bending in coil form. Is it allowed or again we shall have to carry out stabilized HT after solution annealing? Client Spec. asks for solution annealing HT only after bending in coil form. 

Your prompt response on the above shall be highly appreciated.

Thanks & regards,


C. R. GANDHI
(QCM)
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...