Friday, February 28, 2014

[MW:20193] RE: 20190] Mutiple WPS from single PQR

No - not if impacts are required.  Base metal thickness is an essential variable (QW-403.8) and a supplementary essential variable (QW-403.6).  Supplementary essential variable, QW-403.6, takes precedence over QW-403.8 thus limiting the minimum qualified thickness.

 

Does the application for your 2nd WPS require impact testing?  If not then supplementary essential variable QW-403.6 will not apply and you can write a WPS, without impact qualification, based only on QW-403.8 and  QW-451.1 (i.e. 5mm < T < 22mm).

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mahammed javeed
Sent: Thursday, February 27, 2014 5:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:20190] Mutiple WPS from single PQR

 

Gents,

 

I have PQR with impact test requirements and the details are below like this.

 

Base material thickness 11mm with impact test requirements

Process GTAW & SMAW

 

base metail qualified range 11mm- 22mm

 

GTAW process deposited weld metal qualified range 8 mm

SMAW process deposited weld metal qualified range 14mm

 

Now I want to make a WPS for a job of 6mm only using GTAW process, I have found a difficulty in understanding the base metal thickness range qualified. 

 

Can I consider only weld metal deposited thickness range this process and make a WPS?

 

Regards

M. Javeed

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...