[MW:20189] Welding filler material suitable to service temperature minus 196 deg C

Dear Experts,

We have a requirement for welding CF8M cast material to service temperature minus 196 DEG C. this welded component is practically not feasible to be subjected to PWHT.
We find Filler E 316L Mn-15 can be used as it is capable of yielding impact requirement of 60J @minus 196 Deg C.

Is this filler be crack resistant(such as fissures), since this has very low ferrite level less than 1% ?

Please clarify the above.

Thanks,
MANIVANNAN.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...