Dear Experts.

 

My project scope of work is to weld a 24”Split Tee with the temper bead process P-1-TO-P-1 Material  please provide me  a drawing and weld sequence for this type of work.

 

 

 

 

Tony

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...