The hydrotest requirements are given by the largest of:

a)    Design standard requirements (ASME B31.3, ASME VIII, PD 5500, EN 13445, EN 13480, etc.

b)    National pressure equipment regulations.

 

Older – now outdated - Danish regulations required 1.3 x design pressure.

 

ASME typically 1.5 x pd x (fy/fy,t) – fy: Design yield stress at room temperature, fy,t: Design yield stress at design temperature)

(pd is the design pressure)

 

The PED (Pressure Equipment Directive) in Europe as well as EN 13445 and EN 13480 reguire the largest of:

a)    1.43 x Design pressure

b)    1.25 x design pressure x (fy/fy,t). – fy and fy,t as above.

 

In Europe the PED requirements are now implemented in all national regulations.

 

regards

Kristian

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of nishant nair
Sent: 27. april 2013 13:02
To: materials-welding@googlegroups.com
Subject: [MW:17573] Hydrotest pressure criteria

 

Why hydrotest pressure is taken 1.3 times of design pressure? What is the criteria that fixes the term 1.5 times or 1.25 times, etc.???

Thanks in advance,
Nishant nair
Sent from Yahoo! Mail

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...