Dear Ali,
 
Please refer the below for your query
 
Position:
 

QW-203 Limits of Qualified Positions for

Procedures

Unless specifically required otherwise by the welding

variables (QW-250), a qualification in any position qualifies

the procedure for all positions. The welding process

and electrodes must be suitable for use in the positions

permitted by the WPS. A welder or welding operator making

and passing the WPS qualification test is qualified for

the position tested. See QW-301.2.

 

Backing:

 
 

QW-251.1 Types of Variables for Welding

Procedure Specifications (WPS). These variables (listed

for each welding process in tables QW-252 through

QW-265) are subdivided into essential variables, supplementary

essential variables, and nonessential variables

(QW-401). The "Brief of Variables" listed in the tables

are for reference
only.

 

Date: Fri, 26 Apr 2013 11:27:25 +0400
From: mhaskar.aly@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:17560] Welding Position & Backing in PQR

Dear Friends,
Is welding position & backing is the criteria for PQR;
 
Can we  use any position , with or without backing for PQR...and we don't have any restriction on above parameters
 
 
 
Kindly clarify as per ASME SEc IX
 
Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...