Re: [MW:17538] Effect of grain growth in toughness and Softness of a metal

Smaller grain size increases the tensile properties and ductility,and reduce the hardness and creep properties.


On Tue, Apr 23, 2013 at 3:48 PM, Binoy Soman <binoy.spp@daelim.co.kr> wrote:

Thanks Mr. Ghulam for your response,

 

My conclusion is,

 

SLOW COOLING > Grain growth > Coarse grains > high ductility, softness & Low hardness

RAPID COOLING > Fine grains > high hardness

But I think large grain structure shows very low impact strength. So how does the TOUGHNESS increases with increase in grain size. Please explain & correct me if I am wrong.

 

S.Binoy

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ghulam Haider
Sent: Monday, April 22, 2013 10:17 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17510] Effect of grain growth in toughness and Softness of a metal

 

grain size is directly related to the toughness of the material.larger the grain size,more is the toughness of materials. Grain size and hardness are inversely related,i.e smaller the grain size, more is the hardness. Ductility is directly related to the grain size. Grain growth is increase in the grain size..so if the grain size increases,ductility and toughness increase and hardness decreases. And as far as heat treatment is concerned, plz specify what exactly you want to know

regards

Ghulam Haider

final year student

Gik Institute

 

 

From: Binoy Soman <binoy.spp@DAELIM.CO.KR>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, April 22, 2013 3:18 PM
Subject: [MW:17506] Effect of grain growth in toughness and Softness of a metal

 

 

Dear experts,

 

Kindly explain the relation between grain growth, toughness, hardness & ductility. If anybody have some texts which explains the basic changes that happens during heat treatment, please share.

 

S.binoy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Thanks and regards
 
SANU.K.NAIR
QC INSPECTOR
Ph: 0507464738
 
         "Try to be a man with values".                               
 
   It's Possible
  ABUDHABI
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...