Re: [MW:17528] Combined welding process qualification

Hi may I know why do you want I back gouge after you have welded with GTAW. 

Sent from my iPhone

On 23 Apr, 2013, at 3:57 PM, james gerald <gerry_tup@yahoo.com> wrote:

If the GTAW weld is not part of Bend Test / Radiography, then GTAW welder has to be qualified separately.
 
SAW welding operator do not require separate qualification.
 
Thanks & Regards

J.Gerald Jayakumar
00968-99438165
From: Han Kuen Chow <chowhk2013@gmail.com>
To: materials-welding@googlegroups.com 
Sent: Tuesday, April 23, 2013 11:27 AM
Subject: [MW:17520] Combined welding process qualification

Dear Expert,

Could you please give your opinion for following matter?

Combined welding process: GTAW + SAW
Test coupon: Single U
Plate thickness: 20 mm
GTAW - root pass and hot pass (approx. 4 or 5 mm)
SAW - filler pass and capping (approx. 16 mm)
Root to be back gouging and filled with SAW.

Question:
1. Does this welder / welding operator qualify to weld with GTAW and SAW? Root to be back gouging and filled with SAW.


2. Is separate qualification required to qualified this welder / welding operator for GTAW + SAW?




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...